    I have managed to use the Plug and Plate Copy Chrome kit succesfully and will post pictures later. Plating hood and door strikers, I need to add more solution, does this affect the solution that I already have used if I just add more to it? Strikers take alot of abuse, will it peel off as because the plating is so thin?

  • #2
    You can just add more to the existing solution.

    I'm not sure if the plating on strikers will hold up for long.
    --
    Mike Caswell