    Yes it will. The corrosion resistance of chrome (a very porous metal) comes from the nickel plate under it. Copy Chrome is a modified nickel plate.

    Leave a comment:


  • bruce_ventura
    started a topic Corrosion Resistance of Copy Chrome

    Corrosion Resistance of Copy Chrome

    I need to rechrome worn and pitted chrome-plated brass and bronze parts for marine applications. The finished parts must resist corrosion in outdoor salt water environments. Will Copy Chrome resist corrosion as well as chrome plating?