I just ordered some Zincate. Can I still use the Plug in Plate copy chrome kit, if I do the porper steps for emersing the part in a glass container with the wand clapmed to the glass while its emmeresed in the copy chrome solution? After I use the zincate on the aluminum parts.
Leave a comment:
-
You can't brush plate aluminum. You need to Zincate the part, then immersion plate with any of our plating baths.
Leave a comment:
-
Copy Chorme question
Can I chrome aluminum? It doesnt say what alloys I can chrome so I'm confused on this after attempting to chrome some small aluminum parts. Its the plug and plate kit.
EDIT: upon searching the other plating kits I come across the other copy chrome kit and is says I need Zincate Primer for aluminumTags: None