  • cast iron

    i'm trying to hard chrome the inside of a cast iron brake cylinder.
    but i'm getting spots that are not chromed.
    iset the part up in my lay and turned it .002 undersize,iwant to put on approx..007 and grind it back to size.
    i think my amps were right 33 sq in so 50 amps ?
    the spots that don't plate are different sizes and different places,got two of 'em i'm trying to do and both of 'em did the same thing
    can any one help?
    thanks in advance.
    roger

  • #2
    We can help if you open a problem report in our support system. Thanks.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com