  • Stripping gold plate

    I have a question regarding the best way to remove gold plate from a
    brass item. One way would be to reverse the polarity of the
    anode/cathode. My question is: doing this, would brass would be removed
    from the base item and contaminate my gold anode? Is there a better
    way to remove the gold (without losing it like by buffing)?