    I found a hard chrome rectifier, Whit the setint of 100 amp and 10 amp for smaler parts. will this work for a fefteen gal. decorative chrome?
    Than's elboriqua

  • #2
    Chrome requires 1 amp per square inch. Your 100 amp rectifier will plate a part that is approx 100 sq in, regardless of the size of your tanks or the amount of solution.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com