I am thinking about buying a chrome kit and would like to know how long the solutions last. They look like they come in powder form. I was wondering how long after you mix them I will be able to use them.
Announcement
Collapse
No announcement yet.
how long does it keep
Collapse
X
-
They will last for years. Keep them lidded.--