    Greetings all:
    Does anyone know if it is possible to plate nickel over cadmium, and is spot plating feasible?

    Thanks for reading

  • #2
    Re: Plug n plate kit for bathroom faucets ?

    Yes - you need to use a <a href="/alzinc.htm" target="_blank">Non-Acidic nickel bath</a>, otherwise the acidic nickel will corrode the cadmium.

    Sure, you can spot plate with a brush plating system.
    --