    Just the standard anodizing kit at http://www.caswellplating.com/kits/aluminum.htm.

    We can take out the heaters, but it won't save you much money...and some of those heaters are ceramic heaters that get to 220 deg F.

    Leave a comment:


  • 68goat
    started a topic Anodize cost

    Anodize cost

    I have your copy cad 4 gallon system and would like to add an anodizing line. I have a nice lab 10 amp power supply and tank heaters, so what would I need for a 4 gallon system without having to buy the whole kit....