    Re: How much to plug&plate

    About 10 sq feet.

    Yes, you can directly plate steel.

    You can build as much copper as required, the more you plate, the thicker it gets.

    Leave a comment:


  • customjosh
    started a topic How much to plug&plate

    How much to plug&plate

    I was wondering how much surface area the plug&plate copy chrome could handle. Could steel screw heads be done without copper plating first. Also, can very much copper be built up with plug&plate. these kits are very interesting,thanks Josh