    I am setting up the Caswell Copy Cad/Zinc plating system and want to use a muriatic bath right before plating. What ratio or muriatic acid and distilled water should I use for the best results.

    Thanks,
    Allen

  • #2
    10% by volume using distilled water
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      Thanks Jason