    Hi all,

    I have built a small barrel plater to copper plate small 3/4 inch pewter tokens. I am using an acid copper plate solution, but i can't get the copper to stay attached to the token. It just peels off. Any suggestions on how to prep the tokens or anything else that might help?

    Thanks

    Joe

  • #2
    What steps are you taking to prepare the pewter for plating ?
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      sanding and rinsing in tap water.

      Comment


      • #4
        by the way, the solution is sulfuric acid, not cyanide.