Announcement

Collapse
No announcement yet.

Plating over stainless steel

Collapse
X
  • Filter
  • Time
  • Show
Clear All
new posts

  • Plating over stainless steel

    New boy at this.... Purchased plug and plate 2 plate over scratched of faded watch links...... Bought the stainless steel activator, read the instruction, watch the film, and the gold did not take 2 scratches....... What should I have done? Very lost....on what 2 do? Help?

  • #2
    So the gold plated everywhere except for the scratched areas ?
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      Yes,what is the problem? Should I use an abrasive sandpaper to clear area, then try 2 plate......or what?
      Last edited by Samblack; 06-07-2017, 02:52 PM. Reason: Wrong word

      Comment


      • #4
        What were the steps you took to prep the surface before activator and plating ?
        --
        Jason Vanderbroek
        315 946 1213 x116
        www.caswellplating.com

        Comment