    Hi
    I am trying to flash copper plate onto 304 stainless for a Christmas ornament. I have soaked in SP cleaner till it passes the water break, 60 seconds in #4 pickle and then into flash copper tank. The plate has a high luster but no adheasion. If I leave it in tank for 15 minutes it starts to wrinkle and peal off. I tried to activate with HCI for 3 minutes and no change in results. Any help would be greatly appreciated.

    Kelly

  • #2
    try our stainless steel activator SKU# PNPSSACT
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com