    I have been keeping my black nickel in the garage, and it has got very cold over the last few months - I still seem to get decent results though - my question is, is the white crystalline precipitate at the bottom of my plastic tank significant ? Should I warm the solution to redissolve it, or decant the solution off the crystals, and dispose of the crystals safely ?

  • #2
    Warm it up to 110-120 Degrees F and mix it up, it will dissolve.
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      Originally posted by Caswellplating_Jason View Post
      Warm it up to 110-120 Degrees F and mix it up, it will dissolve.
      And it did. Thanks for the help Jason, much appreciated.