    Some while ago I had a chassis for a vintage radio plated in what the man called "old nickel" as it would look more period. It came back silky smooth and dull looking which was perfect. Was wondering what is the difference, apart from looks, in this to 'new nickel' which comes up bright and shinny?

    Ant difference in durability and how is the process different?

    thanks Gary

  • #2
    By "old nickel" Do you mean burnished or matte finished nickel ?
    --