    Hi there, I’ve just started using the bright acid copper plating kit from Caswell and the impeller (propellor) in the aquarium filter that was supplied with the kit broke in 3. Has anyone had trouble of this kind?

    Also I replaced it with a new filter (different brand) and the impeller broke again. I’m stumped as to why, unless the acid is reacting the plastic in the impeller?

    Thanks

  • #2
    Something is getting in the way and breaking them, I cant see 2 pumps, different manufacturers both breaking
    --
    Jason Vanderbroek