    Hello
    i am electroplating with zinc
    small nuts and bolts zinc fine with a dull grey then I can polish to shine.
    but larger items like brake calipers are mostly a shiny copper like finish. Some of the peak areas did get some zinc. Why is this happening?

    5amps. 7 volts
    5% acidic white distilled vinegar
    epsom salt
    sugar
    muriatic acid bath
    water rinse.


    thanks
    chad
    Last edited by stuppenfeld; 09-05-2020, 10:09 AM.

  • #2

    Comment


    • #3
      Wow. What’s the point of having a forum??
      10 views. Nobody has any advice?

      Comment


      • #4
        Can you send me some photos of the Solution and set up ?
        --
        Jason Vanderbroek