I have some old tools that were originally nickel plated. They have become dull and rusty over the years and I would like to refinish them. Do I have to remove the old nickel before plating? Can I plate new nickel over the old nickel (once it is prepped)? Is there a way to polish the old nickel without re-plating?
Announcement
Collapse
No announcement yet.
Need to remove old plating
Collapse
X
-
The best way would be to use the B9 Nickel stripper, then finish and re plate. B9 NICKEL STRIPPER - 2.5 LB - Caswell Inc (caswellplating.com)--