  • Thief of no thief

    Good afternoon, I would like to know if it’s best to plate small pieces with a thief wire on each side of the rack or can I do without. What are the advantages of putting a wire?
    I have done both and had good results, my “go to guy” for my copper tanks tells me I should use them because it will allow me to plate with a stronger current. 🤔
    Any advice or suggestions would be appreciated.
    Thank you.