I called Caswell technical support and was told the shelf life for the Plug N’ Plate silver solution is 4 months? Does this sound correct?
Also, I’d like to ask the forum if I can extend the shelf life by refrigerating or freezing?
By shelf life, I’m referring to after initial opening and using the solution.
Also, I’d like to ask the forum if I can extend the shelf life by refrigerating or freezing?
By shelf life, I’m referring to after initial opening and using the solution.