What's the best way to copper plate solid zinc came used for stained glass? I was thinking of trying to brush plate it. Will the solder used to put the pieces together (60% lead 40% zinc) be plated using the same chemicals? Thanks.
Announcement
Collapse
No announcement yet.
copper plate zinc came for stained glass?
Collapse
X
-
You'll need to treat with Pickle #4 first, then plate with Flash Copper.
See http://www.caswellplating.com/supplies/pickle4.html
and http://www.caswellplating.com/kits/flashcopper.html--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com