Announcement

Collapse
No announcement yet.

Plating voltage/current

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • hparent
    replied
    Re: Plating voltage/current

    Thanks for the info. I will be trying out silver plating as soon as the plating solution arrives (silver on copper).

    hp

    Leave a comment:


  • mcaswell
    replied
    Re: Plating voltage/current

    Volts should be between 4-10. The part will draw the required current itself.

    Leave a comment:


  • hparent
    started a topic Plating voltage/current

    Plating voltage/current

    What is the correct voltage and current level recommended for wand plating silver on copper? I have variable power supply that can be adjusted for voltage level and current limiting.

    hp
Working...