I HAVE STRIPPED WASHED, ACTIVATED BUT STLL HAVE SPOTTING...PLEASE READ MY LAST POST...I HAVE GOT TO FIND A SOLUTION FOR THIS...IF THERE IS NOT ONE I HAVE JUST RUINED A VERY EXPENSIVE MOTORCYCLE....AND ITS ALL I HAVE...THANKS
Announcement
Collapse
No announcement yet.
I AM REALLY DESPERATE...I CAN'T GET THE SPOTS OFF STRIPPED
Collapse
X
-
Well:
First off you have not caused irriplacable damage. I doubt if there is any damage at all. You may have to do some stripping and replating though.
I would call or mail Caswell about the problem. Its hard to say whats going on without seeing or talking to the person. Your solution may be low in gold.
If it came on gradually then thats what I would bet on.
That is if you didnt change any of the proceedure.
48Buick
-
SPOTTING ON MOTORCYCLE
THANKS 44 , AT LEAST IVE NOT RUINED ANYTHING...I KEEP CLEANING, STRIPPING BUFFING AND STILL HAVE SPOTS....NO MATTER WHAT I DO...GOLD IS GOOD QUALITY FROM GOLD TOUCH, IN A GEL FORM...I HAVE STRIPPED SO MANY TIMES THERE CAN'T POSSIBLY BE ANY THING LEFT
Comment
-
Originally posted by 48BuickWell:
First off you have not caused irriplacable damage. I doubt if there is any damage at all. You may have to do some stripping and replating though.
I would call or mail Caswell about the problem. Its hard to say whats going on without seeing or talking to the person. Your solution may be low in gold.
If it came on gradually then thats what I would bet on.
That is if you didnt change any of the proceedure.
48Buick
Comment
Comment