  • motoc
    replied
    Originally posted by 48Buick
    Well:
    First off you have not caused irriplacable damage. I doubt if there is any damage at all. You may have to do some stripping and replating though.
    I would call or mail Caswell about the problem. Its hard to say whats going on without seeing or talking to the person. Your solution may be low in gold.
    If it came on gradually then thats what I would bet on.
    That is if you didnt change any of the proceedure.
    48Buick
    THANKS 48...IVE TRIED EVERYTHING...SPOTS STILL THERE...I HAVE STRIPPED OVER AND OVER...BUFFED...STILL GET SPOTS...GOLD IS GOOD QUALITY FRO GOLD TOUCH INC...GEL TYPE...IVE NEVER HAD THIS PROBLEM BEFORE

    Leave a comment:


  • motoc
    replied
    SPOTTING ON MOTORCYCLE

    THANKS 44 , AT LEAST IVE NOT RUINED ANYTHING...I KEEP CLEANING, STRIPPING BUFFING AND STILL HAVE SPOTS....NO MATTER WHAT I DO...GOLD IS GOOD QUALITY FROM GOLD TOUCH, IN A GEL FORM...I HAVE STRIPPED SO MANY TIMES THERE CAN'T POSSIBLY BE ANY THING LEFT

    Leave a comment:


  • 48Buick
    replied
    Well:
    First off you have not caused irriplacable damage. I doubt if there is any damage at all. You may have to do some stripping and replating though.
    I would call or mail Caswell about the problem. Its hard to say whats going on without seeing or talking to the person. Your solution may be low in gold.
    If it came on gradually then thats what I would bet on.
    That is if you didnt change any of the proceedure.
    48Buick

    Leave a comment: