  • txturbo
    replied
    Re: adding color to ploished stainless steel?

    why not add tint to automotive clear and spray it? Also it might be possible to add tint to GlistenPC.

    Leave a comment:


  • athomas
    replied
    Re: Re: adding color to ploished stainless steel?

    Paint isn't what I want to do. It doesn't have the hardness of the steel, therefore it is more prone to damage and changes the tolerances too much.

    caswell wrote:
    There's always paint....

    Watch our web site in the next month or two. We're working on a new product which might do this for you.

    Leave a comment:


  • mcaswell
    replied
    Re: adding color to ploished stainless steel?

    There's always paint....

    Watch our web site in the next month or two. We're working on a new product which might do this for you.

    Leave a comment:


  • athomas
    started a topic adding color to ploished stainless steel?

    adding color to ploished stainless steel?

    I was wondering if there is any way to add a color to polished stainless steel, similar to the effect of anodizing aluminum. Since anodizing doesn't work on steel, I was wondering if there is another alternative.
Working...
X