  • bhhodges
    replied
    are you going to be plating once a week--month-year?? i plate almost daily so i leave all my anodes,heaters and air supply in place with a semi air tight cover over the tanks.


    if your plating less frequently then pull them,rinse and air dry and reinstall next session.

    if i do pull mine i have a container marked nickel anode rinse/copper anode rinse with distilled water and i use this for make-up for evaporation in the plating tank,then you will have no waste water.


    bill

    Leave a comment:


  • rdanielewski
    started a topic Anodes (cleaning & drying)

    Anodes (cleaning & drying)

    When I'm finished using the anodes can they be rinsed, then hung to dry with bandages left on?