Green slime...
Caswells also sells a green plastic substance that you can paint on the part, plate, and then remove with laquer thinner. I just finished plating some motorcycle parts with it, and will report on my success or failure here in a little while.
Announcement
Collapse
No announcement yet.
What is the best way to mask threads and holes?
Collapse
X
-
any type plastic plugs will work well there is also tape specific for plating you can use to cover threads. i believe caswell sells a kit with various sizes of plugs.
bill
Leave a comment:
-
-
What is the best way to mask threads and holes?
I am about to start plating after weeks of polishing. My first parts have alot of threads and holes that cannot change diameter, and one part is a master cylinder where I don't want to get plating inside. I am using the copy chrome and wanted to know what was resistant to the solutions and the plating. I thought plastic like what is on the buckets would work, not really sure. Thanks in advance.
KennyTags: None
-
Leave a comment: