  • Wildkarrde
    replied
    Thanks Caswell!

    Leave a comment:


  • mcaswell
    replied
    Yes.

    Leave a comment:


  • Wildkarrde
    replied
    And then chrome plate it?

    Leave a comment:


  • mcaswell
    replied
    Silvaspray is a conductive paint, designed to be applied to plastic. You can nickel or acid copper plate it.

    Leave a comment:


  • Wildkarrde
    replied
    So what has replaced it? I'd like to plate some plastic but am not sure what to use.

    Leave a comment:


  • mcaswell
    replied
    We discontinued Silvachrome some time ago.

    Leave a comment:


  • Wildkarrde
    started a topic Silvachrome question

    Silvachrome question

    Hey, where on this site do I purchase Silvachrome? I feel like an idiot trying to find his butt with both hands and a flashlight and not succeeding can someone point me in the right direction please?
    Thx!