Re: electroless plating
Our kits are really designed for hobby plating, not the sort of specifications you seem to require.
You might want to try posting your question on finishing.com.
Good luck!
Announcement
Collapse
No announcement yet.
electroless plating
Collapse
X
-
electroless plating
need to coat holes in a plasstic display. The display is PET mylar, 4 mil thick, the holes are bare, drilled mylar. The entire display has 7 microinches of aluminum on both sides i wish to connect electrically by plating the holes. I can't remove more than 500 Angstroms of aluminum and its ok to clog the hole. Any ideas? Ni or Sn would be ok, electroless plating better than electro since I want a thin layer.Tags: None