I too have seen this "recipe" for a gold plating solution. I actually made some up, and it worked pretty well. BUT, I did get a brown precipitant out of solution when mixed. Anyone know what that might be? I'm thinking it might be elemental sulfer.

Welcome To The Caswell Inc Forums - The Place To Be For Metal Finishing Enthusiasts!
We notice that you are not currently registered on our site, or are not logged in. Registration is FREE and allows you to post questions on our forums, post pictures, access Technical Support, place orders for products and much, much more! Why not take a moment and register? Just click the Register Link above.