    Gents,

    I am using high-build acid copper over a flash copper strike. After I am done sanding down the acid copper, do I need to apply another layer of flash copper over the sanded-down acid copper layer (sandwich the acid copper between flash copper layers) or do I simply continue with the rest of the layers on top ?

    Copy Chrome is going to follow on top.

    Thanks,

    Ares

  • #2
    no you dont need to add another layer of flash copper.