Hi,
Two questions.
Is it possible to plate fasteners in a conductive basket in small lots or does each one need to wired up?
Do new commercial fasteners need to stripped and replated in order to plate a thicker zinc layer for outdoor corrosion resistance or can you just degrease and plate more on?
This is for a '91 Japanese Ford tractor
Thanks
Two questions.
Is it possible to plate fasteners in a conductive basket in small lots or does each one need to wired up?
Do new commercial fasteners need to stripped and replated in order to plate a thicker zinc layer for outdoor corrosion resistance or can you just degrease and plate more on?
This is for a '91 Japanese Ford tractor
Thanks