Hi all,
I pulled a stupid and hooked up reverse polarity on a nickel kit while trying to plate a piece of copper. This covered my nickel anodes with a copper plate.
I stripped off the copper from the anodes. But now my solution seems to be contaminated. Can anyone suggest if I need new solution, or would a high amp plate of a corrugated piece clear it?
Thanks,
Andy
I pulled a stupid and hooked up reverse polarity on a nickel kit while trying to plate a piece of copper. This covered my nickel anodes with a copper plate.
I stripped off the copper from the anodes. But now my solution seems to be contaminated. Can anyone suggest if I need new solution, or would a high amp plate of a corrugated piece clear it?
Thanks,
Andy