    I want to nickel plate my paintball gun but it like 5" long 3" tall 1" wide, what type of plating do i need? (hopfully the cheapest way )

    Cya,
    Intimiadator }
    "Be carefull of the toes you step on today, because they might be conected to the foot that is beating you tomrrow"-Some Dude of Mixed Nutz

  • #2
    Re: Question?

    never mind im going to anodizing. Im pretty new to anodizing I now how to do fades but, how do you do splashes and acid wash?

    Cya,
    Timmy
    "Be carefull of the toes you step on today, because they might be conected to the foot that is beating you tomrrow"-Some Dude of Mixed Nutz

    Comment


    • #3
      Re: Question?

      It's not as complex as you'd think - to get a splash effect, you simply splash the dye on. This is definitely an art form - something that requires a little practice to get good at.

      We suggest you practice techniques on scrap aluminum before trying it out on a production piece.

      Our manual has an overview of some common techniques.
      --