could anyone tell me which kit is best for pot metal. would the electroless kit be better than the copy chrome? I have many parts to do from old juke boxes and would appreciate the help and input.
Announcement
Collapse
No announcement yet.
plating pot metal
Collapse
X
-
The trick is to get Flash Copper on the part first, then it won't matter which finish (electroless or copychrome) you use. Personally I like the results I get with the Electroplated nickel, and the maintenance on the tanks is nearly nothing--unlike electroless.
Please read the extensive posts on plating pot metal. You're in for a real ride.
Kind regards,
Ken