Many of the readers at this forum will have used both CopyChrom and Triple Chrome plating kits and supplies from Caswell.
From and overall viewpoint, what are the pros and cons between CopyChrom and Triple Chrome.
At the moment I seem to be between the 2 products where my intended use is vintage vehicle exteriors parts for the most. One of my concern with the Triple Chrome is the 1amp per sq inch and the limitation this may impose where limited to a 12 volt car battery. In the case of CopyChrom I am concerned about the durability aspect.
The copyChrom is supposed to be "Hard Like Chrome" but I wonder if this is the case.
It is not my intention to chrome plate full vehicle bumpers or grills but I do suspect that I may wish to plate upto maybe 2sq feet.
Your thought on the above would be appreciated.
Jezella
From and overall viewpoint, what are the pros and cons between CopyChrom and Triple Chrome.
At the moment I seem to be between the 2 products where my intended use is vintage vehicle exteriors parts for the most. One of my concern with the Triple Chrome is the 1amp per sq inch and the limitation this may impose where limited to a 12 volt car battery. In the case of CopyChrom I am concerned about the durability aspect.
The copyChrom is supposed to be "Hard Like Chrome" but I wonder if this is the case.
It is not my intention to chrome plate full vehicle bumpers or grills but I do suspect that I may wish to plate upto maybe 2sq feet.
Your thought on the above would be appreciated.
Jezella