Can you chrome plate over the electroless chrome since the electroless chrome is basically a nickel/colbolt solution? thanks
Announcement
Collapse
No announcement yet.
question
Collapse
X
-
Re: question
Yes you can.--
Mike Caswell
Caswell Inc