    It has been suggested that you can dip an aluminum part in nitric acid between zincates to ensure it takes.

    Does anyone know where I can buy nitric acid?

    Should it be diluted 50 percent wtih distilled water?

    Is this a good practice?

  • #2
    I researched this awhile back and stumbled on a few articles that suggested a 60% nitric acid dip prior to zincating, to etch the surface. I have never tried it however. You can probably buy nitric acid at a chemical supplier like daigger.com.

    Be careful when handling the stuff.