    Re: electroless question

    Sure, just don\'t spill any in the spaghetti.

    There aren\'t any hazardous fumes from this kit, although you obviously need to excercise common sense in handling any chemical product.

    Leave a comment:


  • felix
    started a topic electroless question

    electroless question

    Are there any hazardous fumes or can I do this on my kitchen stove?