  • What kind of filter should I use on my chrome bath?

    I have installed a pump system on my chrome bath and I would like to filter it. I need to know if there is a cartridge filter that can handle chromic acid. I can buy a small filter chamber to complete my filtration system. We live out in the country and there is a lot of dust in the air. I want to keep my chrome clean.

    If anyone has an answer, please let me know.

    thanks

    Kelly

  • #2
    Hi:
    You dont want to filter your chrome.
    It may have sediment in it but it will all settle to the bottom. I just use a small bubbler to keep the temp concistant thoughout the bath.
    When I plate I turn the bubbler off.
    48 Buick