I have been looking at your copy chrome and your info says that it is suitable for smaller items. I have some auto bumpers that I would like to plate. They break down into three pieces each, and are very slim. Could I use a longer, flatter bath for the chemicals ? More like an infants bath rather than a deep bucket ? Your help will be appreciated. Chris.
Subject: size of component to be plated
From: caswellplating.com
Date: Fri, 1 Apr 2005 19:12:57 -0500
That will work.
You need something like a planter window box. If you are only plating one side, you could put the anodes on one side and the bumper on the other. Work out how many gallons the tank needs.
Subject: size of component to be plated
From: caswellplating.com
Date: Fri, 1 Apr 2005 19:12:57 -0500
That will work.
You need something like a planter window box. If you are only plating one side, you could put the anodes on one side and the bumper on the other. Work out how many gallons the tank needs.