Announcement

Collapse
No announcement yet.

Mixing the pickle Baths

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Tim1hd
    replied
    I'm from North Canton. I started using Caswell's Copy Chrome kit first and then I moved on to Acid Copper. Right now I'm having great results so I don't plan on moving on to Triple Chroming anytime soon. Thanks again for your help.
    Tim

    Leave a comment:


  • etcc
    replied
    Hmmm

    You're welcome Tim...it's IMPORTANT to know that difference.

    Also...be sure to add the Acid to the water...NEVER water to acid...and stir well while slowly pouring it in...avoid splashes.

    Which part of Ohio are you from?

    I wish you great success in your plating and all you do.

    Leave a comment:


  • Tim1hd
    replied
    Thanks for your help. I had forgot about this post.

    Tim

    Leave a comment:


  • etcc
    replied
    ACID IN COPPER PLATING BATH

    Hi Tim...
    For optimim results...Sulphuric Acid is used as follows...Per Gallon of Acid Copper Plating Bath Solution...
    7.5 Ounces by WEIGHT...or...
    4.1 ounces FLUID.

    Leave a comment:


  • Tim1hd
    started a topic Mixing the pickle Baths

    Mixing the pickle Baths

    When mixing a acid bath. Is the amount of acid used measured by weight or fluid oz.?