Re: cathode hangers
No, copper is safe to use in any bath.
Announcement
Collapse
No announcement yet.
cathode hangers
Collapse
X
-
Re: cathode hangers
I was going to use brass but someone told me that it\'s bad for the baths, but as for the copper will it mess with the chrome bath..
Leave a comment:
-
Re: cathode hangers
For plating, copper works best.
For anodizing, you must use aluminum wire.
Leave a comment:
-
cathode hangers
what kind of wire would be the best one to use to hang my parts from the cathode, that would\'t corrode my baths....Tags: None
Leave a comment: