    Ok Guy\'s, I\'m almost there. One more question. I have the triple chrom plating kit. In the manual it says the mist suppressior, sulfuric acid, and catalyst are already in the catalyst. My question is do I need to add sulfuric acid as the instructions on the bag says, or is it already in the mixture. Thanks for a great site.................Buddy

  • #2
    Re: Mixing chrome solution

    All you have to add is:

    1. chrome powder
    2. catalyst
    3. distilled water

    The sulfuric acid is now pre-mixed with the chrome solution.
    --