    Put some plastic wrap over the opening of the jar and then put the metal lid on (if its metal) That way the lid will be protected from the chemicals and not deteriorate
    48Buick

    Leave a comment:


  • mcaswell
    replied
    Re: Storage?

    What kind of solution?

    Plastic will work fine for most of them. You might want to put chrome in glass, as it will slowly eat away the plastic.

    FYI - Don\'t use metal containers.

    Leave a comment:


  • stevec
    started a topic Storage?

    Storage?

    After I\'m done plating, what can I used to store the plating solution? I\'m pretty certain that a glass jar will work, but I was wondering if a plastic container would work as well?