I thought I was plating copper over nickel and brass (instrument valve) but I now think that it was chrome and brass. Will copper stick properly to chrome plating?
Announcement
Collapse
No announcement yet.
Un-plating Copper
Collapse
X
-
Re: Un-plating Copper
Yes, you could eventually strip the brass, so be careful.
Use a de-plating setup. Switch the polarity, use a GP Plate and muriatic acid.
You\'ll have to strip the chrome first before copper plating. Nothing will plate over chrome.--