Hi. I was wondering if i were to chrome engine parts for waverunners, and my car how would the chrome hold up? How long does it last and will it work on hot engines?
Announcement
Collapse
No announcement yet.
How well doe sthe chrome stand up?
Collapse
X
-
Re: How well doe sthe chrome stand up?
It will discolor/blue very quickly.
Have you ever seen chromed motorcyle exhausts that have blue stains? That is caused by the heat.
We have a product that removes the bluing, but you will be constantly re-polishing with it. See http://www.caswellplating.com/bluejob.html--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
-
Re: How well doe sthe chrome stand up?
Yes. You can clearcoat them with our VHT High Temperature Paint after polishing.
See http://www.caswellplating.com/vht.htm--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com