  • mcaswell
    replied
    Re: CopyCad plating on 62 sq. in. object

    Copy Cad needs 25 milli amps per sq inch of surface being plated. 62 sq\" needs 1.5 amps, so you are under powered by more than 50%

    Leave a comment:


  • mcaswell
    replied
    Re: CopyCad plating on 62 sq. in. object

    Hi Dave:

    We don\'t take support requests on this board. We\'ve set up an online support system for you to use, which allows us to solve problems more efficiently.

    If you click the \"Need Support?\" link below, you\'ll be taken to our support site, where you can use our PRS system to log your problem. A support tech will post a solution shortly after that.

    Thanks!

    Leave a comment:


  • dhillebr
    started a topic CopyCad plating on 62 sq. in. object

    CopyCad plating on 62 sq. in. object

    I\'m trying to plate motorcycle hubs and sprockets with the CopyCad kit. I\'m getting a rough dull gray plate. I tried a 700ma, 1.5 volt supply with no change in results. I am not sure if I should be increasing voltage or amps to get desired results. Small items such as nuts and bolt plate fine.