    I am setting up a tank out of a chemical grade Plastic 55 gallon barrel. And was wondering if a hot water tank heat with a thermastate would work? The electrode on the element is copper. Would this affect any of the tank? ( Looking for a cost effective way to heat 45 gallons ) Any help would be greatly appreciated.
    Thanks jsnow2060

  • #2
    You can't have any metal parts inside the tank. Your copper element would cause major problems.

    Do you have our manual? There is a good section in there on heating up large amounts of solution.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      You didn't say what was going in the tank. Thats very important. Using mains electric heater that are metal could be VERY dangerous.
      --